Has anybody looked into the ceramic cloth that is available for fireproofing?
Newlan2dl@aol.com wrote:
> The HDT of Jeffco the resin we're using is 190 degrees but that is probably
> about 10-20 degrees above what the glass transition temperature is. The
> strength wand modulus will drop off pretty quickly as the heat gets above the
> HDT.
>
> The core of our birds are quite resistant to flame since phenolics are
|
|