Question for you glass fellows.  Yesterday I laid up some cloth on the cowl and it didn't harden.  I put some heat on it with the heat lamp and left it over night and nothing.  This morning I put the heat lamp on it and pulled it off, scraped it and ground the area, wiped it down again with acetone and tried again.  The epoxy is United Resin Corp. Uni-Lam.  The shop is hot water heated with pipe in the floor and this epoxy is supposed to work at room temperature..The ratio by volume is 1 to 3.8,  it has been working ok by using a marked stick in a soup can, but I'm wondering if this ratio is hyper critical.  Any input would be greatly appreciated.  JohnD